Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by.. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
PlastiComp Complet® LGF40-PA66 MT 40% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 505R PC Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 215HPR PBT Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21.. |
|||
Izod Impact, Unnotched | 16.02 J/cm @Temperature 23.0 °C |
30.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 295 PBT Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 310HP PBT PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Izod Impact, Unnotched | 16.02 J/cm @Temperature 23.0 °C |
30.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 312 PBT Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Unreinforced, For compounding only (not for injection molding), Medium viscosity. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Izod Impact, Unnotched | 16.02 J/cm @Temperature 23.0 °C |
30.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific) 325M is a high flow VALOX 325 for restrictive gate tooling (key buttons)This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 745 PBT 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific) LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON PX06419 PA 6 LNP* VERTON* PX06419 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, Structural. |
|||
Izod Impact, Unnotched | 16.02 J/cm | 30.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON PX06419 PA 6 (Asia Pacific) LNP* Verton* PX06419 is a compound based on Nylon 6 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |