Mechanical Properties Metric English Comments
Flexural Strength 296 MPa
42900 psi
ASTM D790
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS)
Information provided by PolyOne
Flexural Strength 296 MPa
42900 psi
ASTM D790
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Strength 296 MPa
42900 psi
ASTM D790
PolyOne Nymax™ GF 1200 A 43 HS Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Flexural Strength 296 MPa

@Temperature 23.0 °C
42900 psi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Flexural Strength 296 MPa
42900 psi
ASTM D790
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Flexural Strength 296 MPa
42900 psi
ASTM D790
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Flexural Strength 296 MPa

@Strain 3.20 %
42900 psi

@Strain 3.20 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 296 MPa
42900 psi
5 mm/min; ISO 178
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Strength 296 MPa
42900 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66
LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive.
Flexural Strength 296 MPa

@Temperature 23.0 °C
42900 psi

@Temperature 73.4 °F
4; ISO 178
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Flexural Strength 296 MPa
42900 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific)
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Flexural Strength 296 MPa
42900 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK
LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu..
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific)
LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s).
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA
LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s).
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON PV007 PA 6
LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural.
Flexural Strength 296 MPa
42900 psi
ASTM F417
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Flexural Strength 296 MPa
42900 psi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
Flexural Strength 296 MPa

@Temperature 23.0 °C
42900 psi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific)
LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber.
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON PX06419 PA 6
LNP* VERTON* PX06419 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, Structural.
Flexural Strength 296 MPa
42900 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON PX06419 PA 6 (Asia Pacific)
LNP* Verton* PX06419 is a compound based on Nylon 6 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Copyright © lookpolymers.com All Rights Reserved