Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp BX06088 SAN (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp BX06088 SAN (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* BX06088 is a compound based on Styrene Acrylonitrile Blend resin containing Carbon Fiber. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Tensile Modulus 6.60 GPa
957 ksi
1 mm/min; ISO 527
Flexural Yield Strength 105 MPa
15200 psi
2 mm/min; ISO 178
Flexural Modulus 6.50 GPa
943 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D 257