Material Notes:
Weight per Epoxide (EEW, g/eq) 185 to 196. Max color is 3.Comments/Applications: Provides excellent heat and chemical resistance especially in post bake or heat cured coatings. Chemically modified bis A epoxy; functionality of 2.3. Se XU GT 259 for solid version of PY 258. Formerly XU MY 252.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 700 - 1100 cP
700 - 1100 cP