3M Scotchcal™ IJ780Cv3 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ IJ780Cv3 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat surfaces, with and without rivets, simple curves, compound curves; Removable with heat and/or chemicalsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 17.2 MPa
>= 2490 psi
Peel Strength 0.701 - 0.877 kN/m
4.00 - 5.00 pli
Adhesion to ABS
0.701 - 1.05 kN/m
4.00 - 6.00 pli
Adhesion to Fruehauf pre-painted panel
0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Acrylic
1.23 - 1.40 kN/m
7.00 - 8.00 pli
Adhesion to Aluminum, etched
1.40 - 1.58 kN/m
8.00 - 9.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 29.0 °C
84.2 °F
Flat surfaces without rivets
29.0 °C
84.2 °F
Curved or corrugated surfaces with rivets
29.0 °C
84.2 °F
Compound curves and/or watercraft
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Flat surfaces without rivets
10.0 °C
50.0 °F
Curved or corrugated surfaces with rivets
16.0 °C
60.8 °F
Compound curves and/or watercraft