Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PF1006HI005 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PF1006HI005 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact Nylon 6 compound containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
50 mm/min; ISO 527
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
50 mm/min; ISO 527
Tensile Modulus 8.00 GPa
1160 ksi
1 mm/min; ISO 527
Flexural Yield Strength 200 MPa
29000 psi
2 mm/min; ISO 178
Flexural Modulus 7.00 GPa
1020 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*4; ISO 180/1U
75.0 kJ/m²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae