Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Tensile Modulus 4.77 GPa
692 ksi
50 mm/min; ASTM D638
Flexural Strength 77.9 MPa
11300 psi
ASTM D790
Flexural Modulus 3.78 GPa
548 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.26 J/cm
7.98 ft-lb/in
ASTM D4812
Users viewing this material also viewed the following: