SABIC Innovative Plastics LNP THERMOCOMP MX00709 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MX00709 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MX00709 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this grade are: Heat Stabilized, UV Stabilized.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 76.0 MPa
11000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.7 %
2.7 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 7.86 GPa
1140 ksi
50 mm/min; ASTM D638
Flexural Strength 123 MPa
17800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.17 GPa
895 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.03 J/cm
1.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 151 °C

@Thickness 3.20 mm
304 °F

@Thickness 0.126 in
unannealed; ASTM D648