Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
5 mm/min; ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
1 mm/min; ISO 527
Flexural Yield Strength 196 MPa
28400 psi
2 mm/min; ISO 178
Flexural Modulus 7.00 GPa
1020 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 280 °C
>= 536 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af