SABIC Innovative Plastics LNP Stat-kon FX99030 PE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Stat-kon FX99030 PE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP * Stat-kon* FX99030 is a compound based on Polyethylene resin containing Carbon Powder. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Elongation at Break 200 %
200 %
50 mm/min; ISO 527
Tensile Modulus 0.200 GPa
29.0 ksi
1 mm/min; ISO 527
Flexural Yield Strength 8.00 MPa
1160 psi
2 mm/min; ISO 178
Flexural Modulus 0.200 GPa
29.0 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D 257