Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Flow 13 g/10 min

@Load 1.20 kg,
Temperature 260 °C
13 g/10 min

@Load 2.65 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa
8270 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 20 %
20 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 89.0 MPa
12900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.79 J/cm
14.6 ft-lb/in
ASTM D256
Dart Drop, Total Energy 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 4.00e+11 ohm
4.00e+11 ohm
ROA; IEC 60093