Mechanical Properties Metric English Comments
Flexural Modulus 2.19 GPa
318 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Flexural Modulus 2.19 GPa
318 ksi
Tangent (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 3514
Description: Black Polycarbonate Polyester AlloyInformation provided by Network Polymers Inc.
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Flexural Modulus 2.19 GPa
318 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East)
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Flexural Modulus 2.19 GPa
318 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS
LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.19 GPa
318 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East)
LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Flexural Modulus 2.19 GPa
318 ksi
ASTM D790
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific)
PPE/HIPS unfilled 80C FR-V2
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT
LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS
PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management.
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
Flexural Modulus 2.19 GPa
318 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS
PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers.
Flexural Modulus 2.19 GPa
318 ksi
ISO 178
Polyram RamTough PZ509 Polycarbonate, Easy Flow, Flame Retardant
Non-transparent polycarbonate, easy flow, flame retardant, for injection molding applications.Information provided by Polyram.
Flexural Modulus 2.19 GPa
318 ksi
ISO 178
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant
Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram.
Flexural Modulus 2.19 GPa
318 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Copyright © lookpolymers.com All Rights Reserved