Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* OEP32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
1.41 g/cc
0.0509 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ISO 527
127 MPa
18400 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
2.0 %
2.0 %
ISO 527
Tensile Modulus 10.56 GPa
1532 ksi
50 mm/min; ASTM D638
10.59 GPa
1536 ksi
1 mm/min; ISO 527
Flexural Strength 193 MPa
28000 psi
ASTM D790
431 MPa
62500 psi
ISO 178
Flexural Modulus 8.54 GPa
1240 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.28 J/cm
8.02 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 23.0 kJ/m²
10.9 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.32
0.32
ASTM D3702 Modified
Coefficient of Friction, Static 0.33
0.33
ASTM D3702 Modified
K (wear) Factor 78.6 x 10-8 mm³/N-M
39.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257