Mechanical Properties Metric English Comments
Tensile Modulus 10.59 GPa
1536 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear (Asia Pacific)
LNP* STAT-KON* OEP32 is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive.
Tensile Modulus 10.59 GPa
1536 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear
LNP STAT-KON* OEP32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.