Material Notes:
LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
ASTM D 638
Elongation at Break 2.1 %
2.1 %
ASTM D 638
Flexural Strength 158 MPa
22900 psi
ASTM D 790
Flexural Modulus 8.26 GPa
1200 ksi
ASTM D 790
Izod Impact, Notched 0.260 J/cm

@Temperature 23.0 °C
0.487 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C

@Thickness 3.20 mm
473 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D 648