Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66
LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific)
LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region.