Material Notes:
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
1.55 g/cc
0.0560 lb/in³
ISO 1183
Moisture Absorption 0.0200 %
0.0200 %
50% RH, 24 hrs; ASTM D570
0.0200 %
0.0200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 121 MPa
17500 psi
ASTM D638
165 MPa
23900 psi
ISO 527
Elongation at Break 0.80 %
0.80 %
ASTM D638
0.80 %
0.80 %
ISO 527
Tensile Modulus 22.95 GPa
3329 ksi
50 mm/min; ASTM D638
26.2 GPa
3800 ksi
1 mm/min; ISO 527
Flexural Strength 253 MPa
36700 psi
ASTM D790
259 MPa
37600 psi
ISO 178
Flexural Modulus 24.54 GPa
3559 ksi
ASTM D790
25.94 GPa
3762 ksi
ISO 178
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.95 J/cm
7.40 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 4.00 J
2.95 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.31
0.31
ASTM D3702 Modified
K (wear) Factor 94.7 x 10-8 mm³/N-M
47.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
269 °C

@Thickness 3.20 mm
516 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: