Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Strength | 259 MPa @Temperature 23.0 °C |
37600 psi @Temperature 73.4 °F |
Conditioned; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Strength | 259 MPa @Temperature 23.0 °C |
37600 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 259 MPa | 37600 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Flexural Strength | 259 MPa | 37600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 259 MPa @Temperature 23.0 °C |
37600 psi @Temperature 73.4 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Strength | 259 MPa @Temperature 23.0 °C |
37600 psi @Temperature 73.4 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI LNP* THERMOCOMP* EC004XXC is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific) LNP* Thermocomp* EC004XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Flexural Strength | 259 MPa | 37600 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 259 MPa | 37600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |