Polymer Property : Flexural Strength = 253 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 253 MPa

@Temperature 23.0 °C
36700 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Flexural Strength 253 MPa
36700 psi
ASTM D790
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Strength 253 MPa
36700 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12
LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant.
Flexural Strength 253 MPa
36700 psi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS
LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA..
Flexural Strength 253 MPa
36700 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Strength 253 MPa

@Temperature 23.0 °C
36700 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Flexural Strength 253 MPa
36700 psi
ASTM D790
Techmer ES HiFill® PA12 GF50 L 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Flexural Strength 253 MPa
36700 psi
ASTM D790
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..