Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Steel Filled
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Water Absorption 0.54 %

@Time 86400 sec
0.54 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
5 mm/min; ISO 527
Tensile Strength, Yield 82.0 MPa
11900 psi
5 mm/min; ISO 527
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
2.2 %
2.2 %
Flexural Strain, break, 2 mm/min; ISO 178
Elongation at Yield 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 7.90 GPa
1150 ksi
1 mm/min; ISO 527
Flexural Strength 103 MPa
14900 psi
2 mm/min; ISO 178
Flexural Yield Strength 116 MPa
16800 psi
2 mm/min; ISO 178
Flexural Modulus 8.20 GPa
1190 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257