SABIC EPS 652 Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC EPS 652 Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS 652 is an expandable polystyrene grade supplied in free-flowing beads, containing pentane (CFC free) as a foaming agent. It is used for fast cycle medium density shape and block molding applications with good surface finish.Typical Applications: EPS 652 is a standard fast cycle grade used for articles with large shape molding and medium density molding.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.0160 - 0.0250 g/cc
0.000578 - 0.000903 lb/in³
Normal range, one pre-expansion
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in