Precision Polymer Engineering E90K Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E90K Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose, peroxide cured, Ethylene Propylene Terpolymer, 85-95 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM D2000/SAE J200 line call out M8CA910, A25, B35, C32, EA14, and F17.Applications: Excellent water and steam resistance with good compression set properties. Improved heat resistance compared to sulphur cured EPDM. Not oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
100
100
°IRHD, +10 change after 70 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
-20% change after 70 hours @ 125°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 60.0 %
60.0 %
-40% change after 70 hours @ 125°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 50 %
50 %
22 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F