Material Notes:
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.Resin Technology Group UV-406 Millenium™ UV Curable AdhesiveHigh clarity, moisture resistant plastic, glass and metal bonder.
Physical Properties Metric English Comments
Viscosity 60 - 100 cP
60 - 100 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Color White