Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 60 - 100 cP @Temperature 25.0 °C |
60 - 100 cP @Temperature 77.0 °F |
Uncured |
Resin Technology Group UV-406 High Clarity, Moisture Resistant, UV Curing Bonder UV 406 is a rapidly curing UV adhesive developed for use in bonding a variety of plastics, glass and metals, where moisture resistance and low shrinkage during cure is critical. Bond strengths on po.. |
|||
Viscosity | 60 - 100 cP | 60 - 100 cP | |
Resin Technology Group UV-406 Millennium™ UV Curable Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Viscosity | 60 cP | 60 cP | |
Resinlab® CYNERGY CA6102 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 60 - 100 cP | 60 - 100 cP | As Supplied |
Heraeus Cleviosâ„¢ P Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P is an antistatic material based on PEDOT:PSS.. |
|||
Viscosity | 60 cP | 60 cP | at shear rate 3000s-1 |
Solvay Chemicals NOCOLOK® Flux Plus Binder Mixture Potassium Fluoroaluminate A preparation of NOCOLOK® Binder, NOCOLOK® Thickener, NOCOLOK® Flux and water to improve adhesion of the flux coating and to reduce flux fall-off and minimize dust formation. CAS-No.: 6030.. |
|||
Viscosity | 60 cP | 60 cP | |
Shin-Etsu Silicones KE-3470 Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 60 - 70 cP | 60 - 70 cP | |
Master Bond Mastersil 773 Fast Curing Low Viscosity Silicone Master Bond MasterSil 773 is a ready-to-use one component ultra-low viscosity silicone elastomer based conformal coating which provides excellent protection to electronic circuitry in high humidity .. |
|||
Viscosity | 60 cP @Temperature 23.0 °C |
60 cP @Temperature 73.4 °F |
|
Master Bond UV11-3 Abrasion Resistant, UV Curable Coating System Master Bond UV11-3 is an extra-hard, super-abrasion resist-radiation curable coating system for plastic substrates. It is a low viscosity, clear, 100% reactive liquid that can be cured readily by ex.. |
|||
Viscosity | 60 cP | 60 cP | |
Loctite® Assure™ 425 Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 60 - 100 cP | 60 - 100 cP | NOV QC 020 |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 60 - 125 cP @Temperature 25.0 °C |
60 - 125 cP @Temperature 77.0 °F |
|
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Viscosity | 60 - 200 cP | 60 - 200 cP | |
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% .. |
|||
Viscosity | 60 - 120 cP | 60 - 120 cP | |
3M Pronto™ CA-4 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting multi-purpose cyan.. |
|||
Viscosity | 60 cP | 60 cP | |
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder A basic solution compatible with most ceramic and metal powders. Excellent binder for producing high temperature protective coatings and refractory and chemically resistant adhesives and patching ma.. |
|||
Viscosity | 60 cP @Temperature 20.0 °C |
60 cP @Temperature 68.0 °F |
|
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC)
(Unverified Data**) IXAN® SGA-1 is a self-adhesive coat for use on aluminium, steel and plastic films, metallised or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti.. |
|||
Viscosity | 60 - 200 cP | 60 - 200 cP | |
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°.. |
|||
Viscosity | 60 - 125 cP @Temperature 25.0 °C |
60 - 125 cP @Temperature 77.0 °F |
Uncured |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Viscosity | 60 cP @Temperature 20.0 °C |
60 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik 75aH Carboxymethylcellulose (CMC) Technical GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conc.. |