Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1015HLFRA Nylon 66, 15% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1015HLFRA Nylon 66, 15% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 66, 15% Glass Filled, Heat Stabilized, Lubricated, RoHS Compliant, Flame RetardantInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 5.100 GPa
739.7 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0 - 5VA

@Thickness 3.00 mm
V-0 - 5VA

@Thickness 0.118 in