Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Proto3000
Trade Name Duraform®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic elastomer material with rubber-like flexibility and functionality.DuraForm FlexSeal Infiltration:FlexSeal fluid infiltration is an easy-to-use method of coloring, strengthening, and sealing DuraForm Flex parts.Two-Part Polyurethane Infiltration:Infiltration with a two-part polyurethane increases Shore A hardness, creates a watertight barrier, and significantly enhances the burst strength.Features: Durable with good tear resistanceVary Shore A hardness without changing materialEasy-to-processGood powder recycle characteristicsGood surface finish and feature detailBenefits:Withstands repeated bending and flexingBuild prototypes that withstand functional testingProduce durable end-use parts without toolingDuraForm® FlexSeal infiltration offers array of colorsPolyurethane infiltration creates watertight barrier and improves burst strengthApplications: Athletic footwear and equipmentGaskets, hoses and sealsSimulate thermoplastic elastomer, cast urethane, silicone and rubber parts“Soft-touch,” overmolded gripsParts requiring rubber-like flexibility and durabilityForm, fit, or functional prototypesParts that require joining with adhesivesComplex production and prototype plastic partsAppropriate for low- to mid-volume rapid manufacturingDuraForm FlexSeal (1 kg containers) is available in these colors:24130-902: Black24131-902: Red24132-902: Yellow24133-902: BLue24136-902: NaturalInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 0.440 g/cc
0.0159 lb/in³
ASTM D4164
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 75
45 - 75
as sintered; ASTM D2240
55 - 80
55 - 80
Infiltrated with flexseal (8-dip process); ASTM D2240
Tensile Strength, Ultimate 1.20 MPa
174 psi
Infiltrated with flexseal (8-dip process); ASTM D638
1.80 MPa
261 psi
as Sintered; ASTM D638
Elongation at Break 110 %
110 %
as sintered; ASTM D638
151 %
151 %
Infiltrated with flexseal (8-dip process); ASTM D638
Tensile Modulus 0.00740 GPa
1.07 ksi
as sintered; ASTM D638
0.00920 GPa
1.33 ksi
Infiltrated with flexseal (8-dip process); ASTM D638
Flexural Modulus 0.00590 GPa
0.856 ksi
as sintered; ASTM D790
0.00780 GPa
1.13 ksi
Infiltrated with flexseal (8-dip process); ASTM D790
Tear Strength 15.1 kN/m
86.3 pli
as sintered; ASTM D624
15.4 kN/m
87.9 pli
Infiltrated with flexseal (8-dip process); ASTM D624
Taber Abrasion, mg/1000 Cycles 83.5

@Load 1.00 kg
83.5

@Load 2.20 lb
CS-17 wheel; ASTM D4060
Thermal Properties Metric English Comments
Melting Point 192 °C
378 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+14 ohm-cm
1.30e+14 ohm-cm
ASTM D257
Surface Resistance 1.10e+14 ohm
1.10e+14 ohm
ASTM D257
Dielectric Constant 1.85

@Frequency 1.00e+6 Hz
1.85

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 1.90 kV/mm
48.3 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Bursting Strength (Straight) 0.076 MPa
Flex Seal Infiltration (25 mm IDx2 mm thickx300 mm long hose)
0.21 MPa
Two-Part Polyurethane Infiltration (25 mm ID x 2 mm thick x 300 mm long hose)