Mechanical Properties Metric English Comments
Tear Strength 15.4 kN/m
87.9 pli
Infiltrated with flexseal (8-dip process); ASTM D624
Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Thermoplastic elastomer material with rubber-like flexibility and functionality.DuraForm FlexSeal Infiltration:FlexSeal fluid infiltration is an easy-to-use method of coloring, strength..
Tear Strength 15.4 kN/m
88.0 pli
Die B
Shin-Etsu Silicones SV-15000U Silicone Rubber
SV15000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat..
Tear Strength 15.4 kN/m
88.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-1000 TPE
Product Description: StarGrip GP 45-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..