Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00740 GPa | 1.07 ksi | as sintered; ASTM D638 |
Proto3000 Duraform® Flex Selective Laser Sintering (SLS®) Prototyping Polymer Description: Thermoplastic elastomer material with rubber-like flexibility and functionality.DuraForm FlexSeal Infiltration:FlexSeal fluid infiltration is an easy-to-use method of coloring, strength.. |
|||
Tensile Modulus | 0.00740 GPa | 1.07 ksi | as sintered; ASTM D638 |
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems Thermoplastic elastomer material with rubber-like flexibility and functionality. For use with all selective laser sintering SLS® systems.ApplicationsAthletic footwear and equipmentGaskets, hoses an.. |