Material Notes:
Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLow viscosity formulationFully developed and tested build stylesBenefits:Produce ABS-like parts without molding or machiningIncrease market opportunities and acceptance for modelsParts produced within tolerance and faithful to CAD dataIncrease system throughputMinimize part cleaning and finishing laborMaximize reliability with no user R&DApplicationsAutomotive interior componentsShort-run production partsElectronic componentsTesting of functional assembliesRigid and durable functional prototypesConcept and marketing modelsAccurate, durable master patterns for urethane castingInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Liquid
1.20 g/cc
0.0434 lb/in³
Solid
Viscosity 155 - 185 cP

@Temperature 30.0 °C
155 - 185 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength at Break 63.0 - 68.0 MPa
9140 - 9860 psi
ASTM D638
Elongation at Break 5.0 - 8.0 %
5.0 - 8.0 %
ASTM D638
Tensile Modulus 3.20 - 3.38 GPa
464 - 490 ksi
ASTM D638
Flexural Strength 88.0 - 110 MPa
12800 - 16000 psi
ASTM D790
Flexural Modulus 2.69 - 3.24 GPa
390 - 470 ksi
ASTM D790
Izod Impact, Notched 0.120 - 0.220 J/cm
0.225 - 0.412 ft-lb/in
ASTM D256
Gardner Impact 1.10 J
0.811 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C

@Temperature 0.000 - 40.0 °C
33.9 µin/in-°F

@Temperature 32.0 - 104 °F
T<Tg; ASTM E831-93
163 µm/m-°C

@Temperature 75.0 - 140 °C
90.6 µin/in-°F

@Temperature 167 - 284 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 58.0 °C
131 - 136 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 53.0 °C
124 - 127 °F
ASTM D648
Glass Transition Temp, Tg 56.0 °C
133 °F
DMA, E"
Descriptive Properties Value Comments
Appearance White
Critical Exposure (Ec) 7.4 mJ/cm2
Penetration Depth (Dp) 5.2 mils