Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V65B Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V65B Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 61-70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
°IRHD; ASTM D1415
69
69
°IRHD, +5 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 9.76 MPa
1420 psi
-20% change after 72 hours @ 250°C; ASTM D412
12.2 MPa
1770 psi
ASTM D412
Elongation at Break 265.5 %
265.5 %
-10% change after 72 hours @ 250°C; ASTM D412
295 %
295 %
ASTM D412
Compression Set 18 %
18 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F