Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.2 MPa | 1770 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | TD, 1 mil; ASTM D882 |
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial .. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | TD, 3 mil; ASTM D882 |
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial .. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | ASTM D412 |
Precision Polymer Engineering V65B Fluoroelastomer Compound Fluoroelastomer Rubber, 61-70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | ASTM D638 |
ExxonMobil LD 513.48 Molding, Extrusion and Compounding Resin
(discontinued **) LD 513.48 is a medium MI, low density polyethylene resin designed for use in compounds and masterbatches where its properties ensure improved processability and uniform dispersion of additives. The.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer Chemraz® 592, a versatile perfluoroelastomer developed with a proprietary filler system, is very resistant to plasma attack. This compound’s durometer allows for some hardware finish incons.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | Crosshead Speed - 20 in/min; ASTM D638 |
LyondellBasell Petrothene® NA860008 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | Crosshead Speed - 20 in/min; ASTM D638 |
LyondellBasell Petrothene® NA860241 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | ASTM D412 |
Teknor Apex APEX® 3310-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | ASTM D412 |
Teknor Apex Vidux® CV-1000-93 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- Injection moldingInformation provided by Teknor Apex Compa.. |
|||
Tensile Strength, Yield | 12.2 MPa | 1770 psi | ASTM D412 |
Teknor Apex APEX® 3201-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |