Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Over-Molding GradeApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
5 sec; ASTM D2240
Tensile Strength, Yield 6.07 MPa
880 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.00 MPa

@Strain 100 %
290 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
3.76 MPa

@Strain 300 %
545 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 570 %
570 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 22.8 kN/m
130 pli
Die C (graves), 20 in/min; ASTM D624
Users viewing this material also viewed the following: