Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Network Polymers Softflex® 0350 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Split; ASTM D624 |
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | >= 22.7 kN/m | >= 130 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 6221 C NAT The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® A 6221 CUV Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B |
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7100-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D470 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning HS II BASE & 10:1, COLORED CATALYST High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored C.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® LS 4-9060 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® S-2 RTV SILICONE RUBBER BASE & CURING AGENT High strength, lower durometer silicone rubber suited for many moldmaking applications. Silastic S-2 is recommended for use with plaster, cement and rigid polyurethane and can be used with polyester.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | B, cured 72 hrs @ RT |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT38-110 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionInjection MoldingPolyOne Fi.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B, Silicone Property; ASTM D624 |
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, gas.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC