Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam® RP81065 HIPS  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam® RP81065 HIPS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.9 MPa

@Thickness 3.17 mm
2450 psi

@Thickness 0.125 in
2"/min speed; ASTM D638
Elongation at Break 50 %

@Thickness 3.17 mm
50 %

@Thickness 0.125 in
2"/min speed; ASTM D638
Flexural Yield Strength 27.9 MPa

@Thickness 3.17 mm
4050 psi

@Thickness 0.125 in
0.2"/min speed; ASTM D790
Flexural Modulus 1.482 GPa

@Thickness 3.17 mm
214.9 ksi

@Thickness 0.125 in
0.2"/min speed; ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256