Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.482 GPa @Thickness 3.17 mm |
214.9 ksi @Thickness 0.125 in |
0.2"/min speed; ASTM D790 |
PolyOne Maxxam® DP 7916-2001 HIPS
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 1.482 GPa @Thickness 3.17 mm |
214.9 ksi @Thickness 0.125 in |
0.2"/min speed; ASTM D790 |
PolyOne Maxxam® RP81065 HIPS
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 1.482 GPa | 214.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc.. |
|||
Flexural Modulus | 1.482 GPa | 214.9 ksi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f.. |
|||
Flexural Modulus | 1.482 GPa | 215.0 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5101M Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Flexural Modulus | 1.482 GPa | 214.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® BK10 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: BK10 is an SBC developed specifically to have enhanced flow capabilities. It offers improved processability and lower cycle times with the optical clar.. |
|||
Flexural Modulus | 1.482 GPa | 214.9 ksi | ASTM D790 |
Chevron Phillips K-Resin® KR01 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC can be processed by injection molding and extrusion into attractive useful parts that have excellent clarity, good toughness, good stiffness, h.. |