PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 sec; ASTM D2240
Tensile Strength, Yield 16.5 MPa
2390 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 310 %
310 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Oxygen Index 24 %

@Thickness 1.91 mm
24 %

@Thickness 0.0752 in
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 7.20e+13 ohm-cm
7.20e+13 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 166 - 177 °C
331 - 351 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 99%
100°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength 96%
100°C, 1.91 mm; 168 hr, UL Standard
Uses Building Wire Insulation
Wire & Cable Applications
Wire Types NMWU