Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0800-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JKC30A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 176 °C | 331 - 349 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y594B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 210 °C | 330 - 410 °F | Average value: 188 °C Grade Count:4 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Melt Temperature | 166 - 188 °C | 330 - 370 °F | Average value: 177 °C Grade Count:3 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8950-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8980-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8999-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9077-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9600-80 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9915-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9950-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3200-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3211-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 14750 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 1601 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 2134N Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Informati.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8542 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8757 Moldings & Extrusions Flexible PVC Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 50898 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 6651 Moldings & Extrusions Flexible PVC A clear molding and extrusion compound with good processing characteristics and good low temperature properties. Formulated to be resistant to fungal and microbial attack.Information provided by Ge.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9812A-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |