PolyOne Geon™ Vinyl Packaging VE0-112 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging VE0-112 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 43.7 MPa
6340 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.46 GPa
357 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
Izod Impact, Notched 8.50 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Profiles