PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 sec; ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 8.27 MPa

@Strain 100 %
1200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 230 %
230 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Features General Purpose
Low Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Exterior Trim
General Purpose