PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhanced resistance at elevated temperatures is needed. MC100 demonstrates ease of processing with excellent thermal stability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 53.4 MPa
7750 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.58 GPa
374 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 3.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
5.81 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C

@Thickness 3.18 mm
217 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 199 - 207 °C
390 - 405 °F
Descriptive Properties Value Comments
Agency Ratings NSF 14
NSF 61
Forms Pellets
Generic Material CPVC
Generic Name Polyvinyl Chloride, Chlorinated (CPVC)
Processing Method Injection Molding
PVC Cell Classification 23447
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Fittings
Users viewing this material also viewed the following: