Mechanical Properties Metric English Comments
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 451 Nylon 6, 50% RH
Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 454 Nylon 6, 50% RH
Injection molding grade. Nylene 454 is the heat stabilized version of 451 recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistanc..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 600 Nylon 6, 50% RH, Extrusion Grade
Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrif..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 601 Nylon 6, 50% RH, Extrusion Grade
Extrusion grade. Nylene 601 is the heat stabilized version of 600 which is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other app..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 607 Nylon 6, 50% RH, Extrusion Grade
Extrusion grade. Nylene 607 is a very high viscosity extrusion resin having an ASTM relative viscosity of 800. Nylene 607 has excellent structural strength, durability, and physical properties. It ..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade
Film Grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recommended for fl..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256-56
Rotuba 870 Ethyl Cellulose
Data provided by the manufacturer.
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G..
Izod Impact, Notched 3.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
5.81 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)
Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D-256
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
Izod Impact, Notched 3.10 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.81 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 114WO PBT Polyester
A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D-256
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla..