Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by.. |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC) Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance.. |
|||
Tensile Strength, Yield | 53.4 MPa | 7750 psi | ASTM D638 |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |