Polymer Property : Melt Temperature = 405 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 188 - 207 °C
370 - 405 °F
PolyOne Geon™ Vinyl Packaging VEO-111 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Melt Temperature 199 - 207 °C
390 - 405 °F
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)
Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance..
Melt Temperature 200 - 207 °C
392 - 405 °F
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC)
Information provided by PolyOne
Melt Temperature 202 - 207 °C
396 - 405 °F
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible P502 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible R5185A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5D05 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible PVC Compound, designed primarily for extruded sheet and tile applications.Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 196 - 207 °C
385 - 405 °F
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **)
High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance..
Melt Temperature 196 - 207 °C
385 - 405 °F
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound  (discontinued **)
Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat..
Melt Temperature 160 - 207 °C
320 - 405 °F
Average value: 188 °C Grade Count:25
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Melt Temperature 157 - 207 °C
315 - 405 °F
Average value: 182 °C Grade Count:6
Overview of materials for PVC/Acrylic Alloy