Material Notes:
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.21 %

@Thickness 3.17 mm
0.21 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Water Absorption at Saturation 1.75 %

@Thickness 3.17 mm
1.75 %

@Thickness 0.125 in
Long-Term Immersion; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength, Ultimate 207 MPa
30000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 317 MPa
46000 psi
ASTM D790
Flexural Modulus 15.9 GPa
2300 ksi
ASTM D790
Compressive Strength 165 MPa
24000 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
425 °F
Unannealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
420 °F
Unannealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Users viewing this material also viewed the following: