PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Carbon Fiber Filled
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0050 cm/cm

@Thickness 3.18 mm
0.0010 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Thickness 3.18 mm
0.010 - 0.030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.7 MPa
11700 psi
5.1 mm/min; ASTM D638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
Type I; ASTM D638
Tensile Modulus 12.1 GPa
1750 ksi
5.1 mm/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
1.3 mm/min; ASTM D790
Flexural Modulus 8.72 GPa
1260 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Features Copolymer
Electrically Conductive
Good Wear Resistance
Semi Crystalline
Filler / Reinforcement Carbon Fiber Reinforcement, 15% Filler by Weight
Forms Pellets
Generic Material Acetal (POM) Copolymer
Generic Name Acetal (POM) Copolymer
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Business Equipment
Electrical/Electronic Applications
Industrial Applications
Printer Parts