Europrene® N OZO 7028 is a blend of acrylonitrile-butadiene copolymer and polyvinyl chloride in the ratio 70/30. The fluxing stage is fully achieved during the mechanical mixing thus providing outstanding resistance against ozone and good oil, abrasion and fire resistance together with an excellent processability.Key Features: Europrene® N OZO 7028 is characterized by an excellent processability in internal and open mixers, high resistance to oils and outstanding fire resistance. This grade represents a good compromise between ozone resistance and low temperature performances. Particularly suitable for extrusion and injection molding applications, this grade could be vulcanized with sulphur based systems or with peroxides.Main Applications: Conveyor belts, safety shoe soles, cable jackets, insulating hoses, industrial and automotive hoses, flooring, fire hoses and all applications where fire and ozone resistance are required together with good flexibility at low temperature.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
ASTM D5668
Mooney Viscosity 75

@Temperature 100 °C
75

@Temperature 212 °F
ASTM D1646
Ash <= 0.50 %
<= 0.50 %
ASTM D5667
Descriptive Properties Value Comments
Acrylonitrile Content 19.5% wt
ASTM D3533
NBR/PVC Ratio, wt/wt 70/30