Armstrong A-701 Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Armstrong Epoxy Adhesives; Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Armstrong A-701 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond strengths and outstanding chemical resistance. Requires elevate cure schedules.Information provided by Ellsworth Adhesives.
Physical Properties Metric English Comments
Viscosity 250000 cP
250000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Tensile Strength, Ultimate 47.2 MPa
6850 psi
after optimum cure
Elongation at Break 1.9 %
1.9 %
Adhesive Bond Strength 65.5 MPa
9500 psi
Steel-Steel; after optimum cure
30.3 MPa

@Temperature -54.4 °C
4400 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
31.0 MPa

@Temperature 82.2 °C
4500 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
40.3 MPa

@Temperature 25.0 °C
5850 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 20.0 °C
29.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 204 °C
400 °F
Glass Transition Temp, Tg 171 °C
340 °F
Processing Properties Metric English Comments
Processing Temperature 204 °C
400 °F
Optimum cure is 1 hr. @ 400°F
Pot Life 99999 min

@Temperature 25.0 °C
99999 min

@Temperature 77.0 °F
Indefinite working life at 25°C (100 g)
Descriptive Properties Value Comments
Color Grey
Mix Ratio 1 Part