Poco Graphite ZEE-2 Ion Implant Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite ZEE-2 Ion Implant Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotropic graphite with a true 1-micron grain size. A unique manufacturing process yields a graphite with elevated hardness and strengths that exhibits reduced wear and particle generation even in the highest energy environments.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Particle Size 1.0 µm
1.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 100
100
Flexural Strength 103 MPa
14900 psi
Compressive Strength 207 MPa
30000 psi
Thermal Properties Metric English Comments
CTE, linear 8.40 µm/m-°C
4.67 µin/in-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00320 ohm-cm
0.00320 ohm-cm
Descriptive Properties Value Comments
Purity 0.999995