Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.40 µm/m-°C | 4.67 µin/in-°F | |
Poco Graphite ZEE-2 Ion Implant Grade Graphite ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro.. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 260 °C |
4.67 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro EG 2020 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 8.40 µm/m-°C | 4.67 µin/in-°F | ASTM D696 |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
CTE, linear | 8.40 µm/m-°C | 4.67 µin/in-°F | ASTM D696 |
LG Chemical LUMIPLAS LD590T Light diffusion ABS Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 1000 °C |
4.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics 99.8% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 1000 °C |
4.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics AP 35 99% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
CTE, linear | 8.40 µm/m-°C | 4.67 µin/in-°F | 30 - 1500°C |
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 1000 °C |
4.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics Alumina Furnaceware ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles.. |
|||
CTE, linear | 8.40 µm/m-°C @Temperature 20.0 - 650 °C |
4.67 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |