Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 4.67 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 8.40 µm/m-°C
4.67 µin/in-°F
Poco Graphite ZEE-2 Ion Implant Grade Graphite
ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro..
CTE, linear 8.40 µm/m-°C

@Temperature 260 °C
4.67 µin/in-°F

@Temperature 500 °F
Fired Thermal Expansion
Ferro EG 2020 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 8.40 µm/m-°C
4.67 µin/in-°F
ASTM D696
LG Chemical LUMIPLAS LD590 Light diffusion ABS
Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
CTE, linear 8.40 µm/m-°C
4.67 µin/in-°F
ASTM D696
LG Chemical LUMIPLAS LD590T Light diffusion ABS
Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 1000 °C
4.67 µin/in-°F

@Temperature 68.0 - 1830 °F
McDanel Advanced Ceramics 99.8% Alumina
Information provided by McDanel Advanced Ceramic Technologies
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 1000 °C
4.67 µin/in-°F

@Temperature 68.0 - 1830 °F
McDanel Advanced Ceramics AP 35 99% Alumina
Information provided by McDanel Advanced Ceramic Technologies
CTE, linear 8.40 µm/m-°C
4.67 µin/in-°F
30 - 1500°C
Zircar Ceramics DAHP Dense Alumina Hearth Plate
ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity ..
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 1000 °C
4.67 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics Alumina Furnaceware
ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles..
CTE, linear 8.40 µm/m-°C

@Temperature 20.0 - 650 °C
4.67 µin/in-°F

@Temperature 68.0 - 1200 °F
Du-Co Ceramics CS-144-L-5 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Copyright © lookpolymers.com All Rights Reserved